Physical | Nominal Value | (English) | Nominal Value | (SI) | Test Method |
Density | 0.919 | g/cm³ | 0.919 | g/cm³ | ASTM D1505 |
Base Density 1 | 0.919 | g/cm³ | 0.919 | g/cm³ | Dow Method |
Melt Index (190°C/2.16 kg) | 3.9 | g/10 min | 3.9 | g/10 min | ASTM D1238 |
Mechanical | Nominal Value | (English) | Nominal Value | (SI) | Test Method |
Tensile Stress (Break) | 1450 | psi | 10.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 540 | % | 540 | % | ISO 527-2 |
Thermal | Nominal Value | (English) | Nominal Value | (SI) | Test Method |
Melting Temperature | 230 | °F | 110 | °C | Dow Method |
Extrusion | Nominal Value | (English) | Nominal Value | (SI) | Test Method |
Draw Down – from 15 g/m² @ 100 m/min 1600 | ft/min | 500 | m/min | Dow Method | |
Neck-in – 25 g/m² @ 100 mpm 5.8 | in | 148.0 | mm | Dow Method |
Specification: LD LAMINATION-DOW-EC7000
|