LL METALLOCENE-ExxonMobil-4536PA
Add to compare
@ Plastic Dealer Ask owner
SKU: LL METALLOCENE-ExxonMobil-4536PA
Categories: LL, LL METALLOCENE
Tags: American, CAST, ExxonMobil, LL, LL METALLOCENE, S
Product Description
Exceed 4536PA is an ethylene 1-hexene copolymer. Films made from Exceed 4536PA have high modulus and tensile strength. These properties together with excellent drawability make this a versatile polymer for mono layer and multi-layer cast film applications. TnPP is not intentionally added to Exceed 4536PA.
General | |||
Availability 1 | • Africa & Middle East | • Asia Pacific | • Europe |
Additive | • Antiblock: No | • Slip: No | • Thermal Stabilizer: Yes |
Applications | • Artificial grass
• Cast Film |
• Diaper Backsheet
• Hygiene film |
|
Revision Date | • 06/03/2020 |
Resin Properties | Typical Value | (English) | Typical Value | (SI) | Test Based On |
Density | 0.936 | g/cm³ | 0.936 | g/cm³ | ASTM D1505 |
Melt Index (190°C/2.16 kg) | 4.5 | g/10 min | 4.5 | g/10 min | ASTM D1238 |
Peak Melting Temperature | 257 | °F | 125 | °C | ExxonMobil Method |
Thermal | Typical Value | (English) | Typical Value | (SI) | Test Based On |
Vicat Softening Temperature | 244 | °F | 118 | °C | ExxonMobil Method |
Film Properties | Typical Value | (English) | Typical Value | (SI) | Test Based On |
Tensile Strength at Yield MD | 2100 | psi | 15 | MPa | ASTM D882 |
Tensile Strength at Yield TD | 2200 | psi | 15 | MPa | ASTM D882 |
Tensile Strength at Break MD | 6200 | psi | 43 | MPa | ASTM D882 |
Tensile Strength at Break TD | 4800 | psi | 33 | MPa | ASTM D882 |
Elongation at Break MD | 580 | % | 580 | % | ASTM D882 |
Elongation at Break TD | 720 | % | 720 | % | ASTM D882 |
Secant Modulus MD – 1% Secant | 54000 | psi | 370 | MPa | ASTM D882 |
Secant Modulus TD – 1% Secant | 58000 | psi | 400 | MPa | ASTM D882 |
Dart Drop Impact | < 60 | g | < 60 | g | ASTM D1709A |
Elmendorf Tear Strength MD | 30 | g | 30 | g | ASTM D1922 |
Elmendorf Tear Strength TD | 110 | g | 110 | g | ASTM D1922 |
Puncture Force | 6 | lbf | 28 | N | ExxonMobil Method |
Puncture Energy | 9.9 | in·lb | 1.1 | J | ExxonMobil Method |
Optical Properties | Typical Value | (English) | Typical Value | (SI) | Test Based On |
Gloss (45°) | 67 | 67 | ASTM D2457 | ||
Haze | 8.6 | % | 8.6 | % | ASTM D1003 |
Specification: LL METALLOCENE-ExxonMobil-4536PA
|