Product Description
Extrusion- and injection molding grade; with special UV stabilizers; very good hydrolysis and microbial resistance; good low-temperature flexibility; free from plasticizers; high moisture vapor transmission rate; Application; breathable films; Films; Sports shoe soles; hard – soft systems
| Physical | Nominal Value Unit | Test Method |
| Density | 1060 kg/m³ | ISO 1183 4 |
| Mechanical | Nominal Value Unit | Test Method |
| Tensile Stress 5
Break, 23°C |
26.8 MPa |
DIN 53504 |
| 100% Strain, 23°C
300% Strain, 23°C |
2.90 MPa
5.50 MPa |
|
| Tensile Strain 5 (Break, 23°C) | 790 % | DIN 53504 |
| Abrasion Resistance (23°C) | 69.0 mm³ | ISO 4649 |
| Tensile Storage Modulus
-20°C |
125 MPa |
ISO 6721-1,-4 |
| 20°C
60°C |
11.0 MPa
9.00 MPa |
|
| Elastomers | Nominal Value Unit | Test Method |
| Tear Strength 6 (23°C) | 39 kN/m | ISO 34-1 |
| Compression Set
23°C, 72 hr |
22 % |
ISO 815 |
| 70°C, 24 hr | 49 % | |
| Impact | Nominal Value Unit | Test Method |
| Impact Resilience (23°C) | 63 % | ISO 4662 |
| Hardness | Nominal Value Unit | Test Method |
| Shore Hardness (Shore A, 3 sec) | 70 | ISO 868 4 |
Injection Nominal Value Unit
Drying Temperature < 80.0 °C
Processing (Melt) Temp 190 to 210 °C
Mold Temperature 20.0 to 40.0 °C
Extrusion Nominal Value Unit
Drying Temperature < 80.0 °C
Melt Temperature 175 to 210 °C