ASTM Data | |||
Mold Shrinkage, MD | 0.004 | mm/mm | ASTM D 955 |
Density, 73°F | 1600 | kg/m³ | ASTM D 792 |
Rheological properties | dry / cond | Unit | Test Standard |
ISO Data | |||
Melt volume-flow rate, MVR | 25 / * | cm³/10min | ISO 1133 |
Temperature | 360 / * | °C | – |
Load | 10 / * | kg | – |
Molding shrinkage, parallel | 0.3 / * | % | ISO 294-4, 2577 |
Molding shrinkage, normal | 0.6 / * | % | ISO 294-4, 2577 |
Mechanical Properties | dry / cond | Unit | Test Standard |
ISO Data | |||
Tensile Modulus | – / 9800 | MPa | ISO 527 |
Stress at Break | – / 150 | MPa | ISO 527 |
Strain at Break | – / 2.3 | % | ISO 527 |
Tensile Creep Modulus, 1h | * / 9000 | MPa | ISO 899-1 |
Impact Strength (Charpy), +23°C | – / 55 | kJ/m² | ISO 179/1eU |
Impact Strength (Charpy), -30°C | – / 60 | kJ/m² | ISO 179/1eU |
Notched Impact Strength (Charpy), +23°C | – / 10 | kJ/m² | ISO 179/1eA |
Notched Impact Strength (Charpy), -30°C | – / 9.5 | kJ/m² | ISO 179/1eA |
ASTM Data | |||
Tensile Strength at Break | 140 / – | MPa | ASTM D 638 |
Elongation at Break | 1.9 / – | % | ASTM D 638 |
Flexural Modulus | 9722 / – | MPa | ASTM D 790 |
Notched Impact Strength (Izod), 1/8 in | 10 / – | J/m | ASTM D 256 |
Thermal Properties | dry / cond | Unit | Test Standard |
ISO Data | |||
Glass Transition Temperature (10°C/min) | 225 / * | °C | ISO 11357-1/-2 |
Temp. of deflection under load (1.80 MPa) | 223 / * | °C | ISO 75-1/-2 |
Temp. of deflection under load (0.45 MPa) | 224 / * | °C | ISO 75-1/-2 |
Vicat softening temperature, 50°C/h 50N | 217 / * | °C | ISO 306 |
Coeff. of Linear Therm. Expansion, parallel | 15 / * | E-6/K | ISO 11359-1/-2 |
Coeff. of Linear Therm. Expansion, normal | 45 / * | E-6/K | ISO 11359-1/-2 |
Burning Behav. at 1.5 mm Nom. Thickn. | V-0 / * | class | UL 94 |
Thickness tested | 1.5 / * | mm | – |
UL recognition | yes / * | – | – |
Burning Behav. at thickness h | V-0 / * | class | UL 94 |
Thickness tested | 3.0 / * | mm | – |
UL recognition | yes / * | – | – |
Oxygen index | 47.3 / * | % | ISO 4589-1/-2 |
ASTM Data | |||
Coefficient of Thermal Expansion, TD | 40 | E-6/K | ASTM D 696 |
DTUL @ 66 psi | 215 | °C | ASTM D 648 |
DTUL @ 264 psi | 212 | °C | ASTM D 648 |
Electrical Properties | dry / cond | Unit | Test Standard |
ISO Data | |||
Relative permittivity, 100Hz | – / 4.3 | – | IEC 62631-2-1 |
Relative permittivity, 1MHz | – / 4.3 | – | IEC 62631-2-1 |
Dissipation Factor, 100Hz | – / 20 | E-4 | IEC 62631-2-1 |
Dissipation Factor, 1MHz | – / 100 | E-4 | IEC 62631-2-1 |
Volume Resistivity | – / >1E13 | Ohm*m | IEC 62631-3-1 |
Surface Resistivity | * / >1E15 | Ohm | IEC 62631-3-2 |
Electric Strength | – / 37 | kV/mm | IEC 60243-1 |
Comparative tracking index | – / 125 | – | IEC 60112 |
Specification: PESU+GF-BASF-Ultrason E2010 G6 UN
|
There are no reviews yet.